NDT Solution
[ click
here for the NDT Solution Archive ]
Observations on Magnetic Wall
Measurements of Coiled Oilfield Tubing
Figure
4-5
Figure 4 - Tangential surface field
strength versus tube wall thickness at 2.97 A (upper plot is 100 grade, lower
plot is 90 grade).
[ Back to February '04 NDT Solution
]
Figure 5 - Tangential surface field
strength versus tube wall thickness at 3.47 A.
[ Back to February '04 NDT Solution
]
Copyright © 2004 by
the American Society for Nondestructive Testing, Inc. All rights reserved.
Copyright © 2008 by the American Society for Nondestructive Testing, Inc. ASNT is not responsible for the authenticity or accuracy of information herein. Published opinions and statements do not necessarily reflect the opinion of ASNT. Products or services that are advertised or mentioned do not carry the endorsement or recommendation of ASNT.
IRRSP, NDT Handbook, The NDT Technician and www.asnt.org are trademarks of the American Society for Nondestructive Testing, Inc. ACCP, ASNT, Level III Study Guide, Materials Evaluation, Nondestructive Testing Handbook, Research in Nondestructive Evaluation and RNDE are registered trademarks of the American Society for Nondestructive Testing, Inc.
ASNT exists to create a safer world by promoting the profession and technologies
of nondestructive testing. |