8-10
Figure 8 - Image of perpendicular crack
with liquid penetrant results overlay.
[ Back to September '04 NDT Solution
]
Figure 9 - Crack at 58.5 m (192 ft.),
middle horizontal weld: (a) as found; (b) after bleed out.
[ Back to September '04 NDT Solution
]
Figure 10 - Ultrasonic image of crack
58.5 m (192 ft), middle horizontal weld. The through wall part of the
crack is shown in the boxed area. The ultrasonic image has been rotated to the
same orientation as in the visual image (Figure 9).
[ Back to September '04 NDT Solution
]
Copyright © 2004 by
the American Society for Nondestructive Testing, Inc. All rights reserved.
Copyright © 2008 by the American Society for Nondestructive Testing, Inc. ASNT is not responsible for the authenticity or accuracy of information herein. Published opinions and statements do not necessarily reflect the opinion of ASNT. Products or services that are advertised or mentioned do not carry the endorsement or recommendation of ASNT.
IRRSP, NDT Handbook, The NDT Technician and www.asnt.org are trademarks of the American Society for Nondestructive Testing, Inc. ACCP, ASNT, Level III Study Guide, Materials Evaluation, Nondestructive Testing Handbook, Research in Nondestructive Evaluation and RNDE are registered trademarks of the American Society for Nondestructive Testing, Inc.
ASNT exists to create a safer world by promoting the profession and technologies
of nondestructive testing. |